Boehler L625 has high strength up to 980 deg C (1800 deg F) with good resistance to oxidizing atmospheres. It is resistant to a wide variety of corrosive media and to stress-corrosion cracking, pitting, and intergranular attack. It has good fabricability characteristics. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: Ni-645. Producer or source: Böhler-Uddeholm Specialty Metals Inc.